Melt Infiltration Casting of Alumina Silicon Carbide and Boron Carbide
Reinforced Aluminum Matrix Composites
Author(s): Ali Kalkanli, Tayfun Durmaz, Ayse Kalemtas and Gursoy ArslanAli Kalkanli, Tayfun Durmaz, Ayse Kalemtas and Gursoy Arslan
This paper discuss the effect of processing details such as particle size, sintering temperature, preform preparation, aluminum alloy characteristics and melt temperature on the final mechanical properties of ceramic phase reinforced metal matrix composites. Since alloy composition was determined as 7075 and 7085 optimum solutionizing and ageing temperatures were studied to determine maximum hardness values. For only 7085 alloy best solutionizing temperature is 465°C and for 7075 alloy the maximum hardness achived as 178 BHN after heat treatment at 475°C. Alloys were heat treated for recystallization after hot rolling grain size were measured as 100-120 μm for 7085 alloy matrix. Various sintering temperatures were used for preform preparation such as 1300-1450°C. In 85% Al2O3 reinforced 7085 Alloy based MMCs preforms sintered at 1450°C high hardness values were achi.. Read More»
DOI:
10.4172/2169-0022.1000357
Journal of Material Sciences & Engineering received 3677 citations as per Google Scholar report